{"title":"WELD CRACK DETECTION KIT \u0026 SPRAY","description":"\u003cp\u003eWeld crack \u0026amp; flaw detection kits in the form of dye penetrant, developer \u0026amp; cleaner form a key plank in the non-destructive testing of welds. Where weld defects are not visible to the eye, the detection sprays give a visual guide to where any cracks \u0026amp; imperfections may lie.\u003c\/p\u003e\n\u003ch3\u003eHow does a weld crack detection system work?\u003c\/h3\u003e\n\u003col\u003e\n\u003cli\u003eClean the surface of the material with \u003ca href=\"https:\/\/www.fosterindustrial.co.uk\/chemetall-s76-cleaner\"\u003ecleaner\u003c\/a\u003e and wipe thoroughly with a lint free cloth to remove surface contamination. Parts must be at an ambient temperature, before penetrant is applied. Spray the area liberally with the penetrant and allow 10 minutes contact time. If very fine defects are to be located, extend the contact time to 20 minutes.\u003c\/li\u003e\n\u003cli\u003eClean off the \u003ca href=\"https:\/\/www.fosterindustrial.co.uk\/chemetall-240-checkmor-penetrant\"\u003epenetrant \u003c\/a\u003eby wiping with a lint free cloth. Complete the removal using a lint free cloth soaked in cleaner. Clean \u0026amp; dry thoroughly.\u003cbr\u003e\n\u003c\/li\u003e\n\u003cli\u003eApply \u003ca href=\"https:\/\/www.fosterindustrial.co.uk\/chemetall-ld8-developer\"\u003e\u003cspan style=\"font-size: 0.875rem;\"\u003edeveloper\u003c\/span\u003e\u003c\/a\u003e\u003cspan style=\"font-size: 0.875rem;\"\u003e\u003ca href=\"https:\/\/www.fosterindustrial.co.uk\/chemetall-ld8-developer\"\u003e \u003c\/a\u003eby spraying on an even film at least 10 minutes before inspecting for fine defects. Inspect in daylight or under ultravoilet light as appropriate. The system will show continuous lines or pin points where there are cracks or porosity.\u003c\/span\u003e\n\u003c\/li\u003e\n\u003c\/ol\u003e\n\u003ch3\u003eWhy are the pros \u0026amp; cons of using weld crack detection sprays over radiography when non-destructive testing?\u003c\/h3\u003e\n\u003col\u003e\n\u003cli\u003eUnlike ultrasonic \u0026amp; radiographic testing, dye penetrant inspection (DPI) sprays require minimal investment. They can be deployed with minimal training and can be quickly applied.\u003c\/li\u003e\n\u003cli\u003eCrack \u0026amp; defects become visible under normal lighting, with no waiting period for data analysis. The contrasting colour of the developer against the penetrant makes even the smallest cracks visible to the naked eye. With no power needed, Dye penetrant inspection kits are a vital component of a welding inspector armoury, allowing for quick \u0026amp; easy site inspection and testing.\u003c\/li\u003e\n\u003cli\u003eRadiography, on the other hand, provides a more comprehensive and detailed inspection capability, detecting both surface and subsurface defects. The recordable data given rules out subjectivity and offers a QA department auditable records.\u003c\/li\u003e\n\u003cli\u003eIn essence, X-ray offers you a more comprehensive look at a welds integrity and won't be affected by surface paint or chemicals on the material surface.\u003c\/li\u003e\n\u003c\/ol\u003e\n\u003cp\u003e \u003c\/p\u003e","products":[{"product_id":"jac-2-cleaner","title":"JAC-2 Cleaner Aerosol 400 ml","description":"\u003cp class=\"large\"\u003e\u003cstrong\u003eJAC 2 dye penetrant cleaner \u0026amp; degreaser from Johnson \u0026amp; Allen.\u003c\/strong\u003e\u003c\/p\u003e\n\u003cul\u003e\n\u003cli\u003eCleans grease \u0026amp; dirt from the work piece, prior to the application of penetrant.\u003c\/li\u003e\n\u003cli class=\"large\"\u003eThen used as a Penetrant Remover, cleaner being applied by impregnating a lint free cloth and then wiping.\u003c\/li\u003e\n\u003cli\u003eUtlised during an inspection process, JAC 2 is applied by impregnating a lint free cloth to wipe away excess penetrant, prior to developer application.\u003c\/li\u003e\n\u003cli\u003e400 ml tin\u003c\/li\u003e\n\u003c\/ul\u003e","brand":"Foster Industrial","offers":[{"title":"Default Title","offer_id":52834513420619,"sku":"52210","price":19.67,"currency_code":"GBP","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0944\/6994\/7723\/files\/52210_2.jpg?v=1752149935"},{"product_id":"super-six-cleaner","title":"Super 6 Weld Crack Cleaner -300 ml","description":"\u003cp class=\"large\"\u003e\u003cstrong\u003e.Super 6 Crack Detector Cleaner is an advanced, industry grade cleaner that uses powerful enzymes to break down and remove tough contaminants from hard surfaces\u003c\/strong\u003e\u003c\/p\u003e\n\u003cul\u003e\n\u003cli\u003eCleans oil \u0026amp; grease form work piece prior to application of penetrant and developer.\u003c\/li\u003e\n\u003cli\u003eNon-toxic and works at an unprecedented speed of up to 70% faster, making it ideal for tough jobs and stubborn stains\u003c\/li\u003e\n\u003cli\u003eSuper 6 Weld crack used in three part weld crack detection kit.\u003c\/li\u003e\n\u003cli\u003e300ml can\u003c\/li\u003e\n\u003c\/ul\u003e","brand":"Foster Industrial","offers":[{"title":"Default Title","offer_id":52834515353931,"sku":"522100","price":5.85,"currency_code":"GBP","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0944\/6994\/7723\/files\/522100d.jpg?v=1752149943"},{"product_id":"jap-penetrant","title":"JAP Penetrant Aerosol 400 ml","description":"\u003cp class=\"large\"\u003e\u003cstrong\u003eJAP penetrant from Johnson \u0026amp; Allen is a solvent removable red penetrant \u003c\/strong\u003e\u003c\/p\u003e\n\u003cul\u003e\n\u003cli\u003ePart 2 of a weld crack detection kit.\u003c\/li\u003e\n\u003cli\u003eUsed to locate open flaws on a surface, along with cracks \u0026amp; weld porosity\u003c\/li\u003e\n\u003cli\u003e400 ml tin.\u003c\/li\u003e\n\u003c\/ul\u003e","brand":"Foster Industrial","offers":[{"title":"Default Title","offer_id":52834519777611,"sku":"52211","price":21.89,"currency_code":"GBP","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0944\/6994\/7723\/files\/52211_1.jpg?v=1752149952"},{"product_id":"super-six-penetrant","title":"Super 6 Weld Crack Penetrant -300 ml","description":"\u003cp class=\"large\"\u003e\u003cstrong\u003eSuper 6 weld crack Penetrant in 300 ml aerosol \u003c\/strong\u003e\u003c\/p\u003e\n\u003cul\u003e\n\u003cli\u003eSprayed onto work piece and allowed to penetrate for 15 minutes.\u003c\/li\u003e\n\u003cli\u003ePart of 3 weld crack penetration kit\u003c\/li\u003e\n\u003cli\u003eDeveloper is then applied \u0026amp; cracks appear as red on white background.\u003c\/li\u003e\n\u003cli\u003e300ml can\u003c\/li\u003e\n\u003c\/ul\u003e","brand":"Foster Industrial","offers":[{"title":"Default Title","offer_id":52834522923339,"sku":"522110","price":5.5,"currency_code":"GBP","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0944\/6994\/7723\/files\/522110c.jpg?v=1752149960"},{"product_id":"jad-2-developer","title":"JAD-2 Developer Aerosol 400 ml","description":"\u003cp class=\"large\"\u003e\u003cstrong\u003eJAD dye penetrant developer from Johnson \u0026amp; Allen is a quick drying white liquid develepor.\u003c\/strong\u003e\u003c\/p\u003e\n\u003cul\u003e\n\u003cli class=\"large\"\u003eJAD Developer is applied after penetrant removal.\u003c\/li\u003e\n\u003cli class=\"large\"\u003eLarge defects will usually appear almost instantly.\u003c\/li\u003e\n\u003cli class=\"large\"\u003eSmaller fine indications may take up to 10 minutes development time.\u003c\/li\u003e\n\u003cli class=\"large\"\u003eExamine under white light of 500Lux or more for Red Penetrants or 365nm nominal peak UV Light.\u003c\/li\u003e\n\u003cli\u003ePart 3 of a weld crack detection kit.\u003c\/li\u003e\n\u003cli\u003eSuitable for use with red \u0026amp; flourescent penetrants.\u003c\/li\u003e\n\u003cli\u003e400 ml tin\u003c\/li\u003e\n\u003c\/ul\u003e","brand":"Foster Industrial","offers":[{"title":"Default Title","offer_id":52834528919883,"sku":"52212","price":16.65,"currency_code":"GBP","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0944\/6994\/7723\/files\/52212_1.jpg?v=1752149968"},{"product_id":"super-six-crack-developer","title":"Super 6 Weld Crack Developer -300 ml","description":"\u003cp class=\"large\"\u003e\u003cstrong\u003eSuper 6 Crack Detector Developer is a high performance, industry grade product designed to detect the smallest of cracks and flaws in pipes and metals.\u003c\/strong\u003e  \u003c\/p\u003e\n\u003cul\u003e\n\u003cli\u003eDeveloper applied after penetrant \u0026amp; cracks appear as red on a white background.\u003c\/li\u003e\n\u003cli\u003eThis crack detector developer is formulated to give fast, accurate results, performing flawlessly even under tough condition.\u003c\/li\u003e\n\u003cli\u003eOffers superior coverage and is the perfect tool for ensuring the highest quality of work.\u003c\/li\u003e\n\u003cli\u003e300ml can.\u003c\/li\u003e\n\u003cli\u003ePart of three part Super 6 weld crack detection kit.\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003cp\u003e \u003c\/p\u003e","brand":"Foster Industrial","offers":[{"title":"Default Title","offer_id":52834532229451,"sku":"522120","price":5.53,"currency_code":"GBP","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0944\/6994\/7723\/files\/522120c.jpg?v=1752149976"},{"product_id":"tygris-galv-spray","title":"Tygris Bright Zinc Galv Spray 400ml R224","description":"\u003cp class=\"large\"\u003e\u003cstrong\u003eTygris bright zinc Galv aerosol spray is utilised for Cosmetic finishing and protection of galvanised steel, where the part has been welded or cut.\u003c\/strong\u003e\u003c\/p\u003e\n\u003cul\u003e\n\u003cli\u003eZinc content assists in prevention of corrosion\u003c\/li\u003e\n\u003cli\u003eResistant to weathering\u003c\/li\u003e\n\u003cli\u003eGreat heat resistance\u003c\/li\u003e\n\u003cli\u003eAluminium powder gives a bright finish to assist with blend with existing coatings.\u003c\/li\u003e\n\u003cli\u003eExcellent adhesion to clean prepared metal\u003c\/li\u003e\n\u003cli\u003eQuick drying, no secondary curing necessary.\u003c\/li\u003e\n\u003cli\u003eSuitable for welding through\u003c\/li\u003e\n\u003cli\u003e400ml tin.\u003c\/li\u003e\n\u003c\/ul\u003e","brand":"Foster Industrial","offers":[{"title":"Default Title","offer_id":52834538881355,"sku":"52231","price":7.6,"currency_code":"GBP","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0944\/6994\/7723\/files\/52231_1_1.jpg?v=1752149985"},{"product_id":"gas-leak-detector","title":"Super Six Gas Leak Detector- 300 ml","description":"\u003cp class=\"large\"\u003e\u003cstrong\u003eSupersix Gas Leak Detector in aerosol form\u003c\/strong\u003e\u003c\/p\u003e\n\u003cul\u003e\n\u003cli\u003eProduces a microporous stable foam which indicates the postion of the smallest leak instantly.\u003c\/li\u003e\n\u003cli\u003eNon toxic.\u003c\/li\u003e\n\u003cli\u003eNon corrosive.\u003c\/li\u003e\n\u003cli\u003eBio degradeable.\u003c\/li\u003e\n\u003cli\u003e300ml aerosol\u003c\/li\u003e\n\u003c\/ul\u003e","brand":"Foster Industrial","offers":[{"title":"Default Title","offer_id":52834550153547,"sku":"52237","price":9.07,"currency_code":"GBP","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0944\/6994\/7723\/files\/52237_1.jpg?v=1752149993"},{"product_id":"chemetall-s76-cleaner","title":"Chemetall S76 Cleaner","description":"\u003cp class=\"large\"\u003e\u003cstrong\u003eChemetall S76 is a colourless solvent based penetrant remover.\u003c\/strong\u003e\u003c\/p\u003e\n\u003cul\u003e\n\u003cli\u003eS76 is predominately utilised to remove both visible red dye and fluorescent penetrants.\u003c\/li\u003e\n\u003cli\u003eAlso used as a solvent precleaner prior to the penetrant application for the removal of oil and greases.\u003c\/li\u003e\n\u003c\/ul\u003e","brand":"Foster Industrial","offers":[{"title":"Default Title","offer_id":52836811637067,"sku":"522101","price":14.0,"currency_code":"GBP","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0944\/6994\/7723\/files\/522101_2.jpg?v=1752153025"},{"product_id":"chemetall-240-checkmor-penetrant","title":"Chemetall 240 Checkmor Penetrant","description":"\u003cp class=\"large\"\u003e\u003cstrong\u003eInnovative weld crack penetrant with improved washing characteristics.\u003c\/strong\u003e\u003c\/p\u003e\n\u003cul\u003e\n\u003cli\u003eCheckmor 240 is a new generation water washable colour contrast penetrant which is widely utlised in many industries for the detection of defects which are open to the surface of non porous parts.\u003c\/li\u003e\n\u003cli\u003eThe main characteristic advantage of this penetrant is its dark red colour which allows easy control and monitoring of the washing process.\u003c\/li\u003e\n\u003c\/ul\u003e","brand":"Foster Industrial","offers":[{"title":"Default Title","offer_id":52836819370315,"sku":"522111","price":13.76,"currency_code":"GBP","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0944\/6994\/7723\/files\/522111_2.jpg?v=1752153032"},{"product_id":"chemetall-ld8-developer","title":"Chemetall LD8 Developer","description":"\u003cp\u003e\u003cstrong\u003eChemetall Xmor LD8 is a liquid suspension of white powder in a quick drying solvent with low sulphur, alkali metal content \u0026amp; halogen.\u003c\/strong\u003e\u003c\/p\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cspan style=\"color: #333333; font-family: 'Open Sans', 'Helvetica Neue', Helvetica, Arial, sans-serif; font-size: 14px;\"\u003eUsed in non destructive testing of welds, casts \u0026amp; forged parts\u003c\/span\u003e\u003cstrong style=\"color: #333333; font-family: 'Open Sans', 'Helvetica Neue', Helvetica, Arial, sans-serif; font-size: 14px;\"\u003e.\u003c\/strong\u003e\n\u003c\/li\u003e\n\u003c\/ul\u003e","brand":"Foster Industrial","offers":[{"title":"Default Title","offer_id":52836823335243,"sku":"522122","price":15.81,"currency_code":"GBP","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0944\/6994\/7723\/files\/522122.png?v=1752153039"},{"product_id":"neopaint-npt16-white-background-paint","title":"Neopaint NPT16 White Background Paint","description":"\u003cp class=\"large\"\u003e\u003cstrong\u003eNeopaint is a white contrast aid paint that has been specifically formulated for use in magnetic particle inspection.\u003c\/strong\u003e\u003c\/p\u003e\n\u003cul\u003e\n\u003cli\u003eDries in under 2 minutes\u003c\/li\u003e\n\u003cli\u003ePerfect for use with aqueous and hydrocarbon based consumable products\u003c\/li\u003e\n\u003cli\u003ePropels at a ratio far superior to liquid propellants like Butane\u003c\/li\u003e\n\u003cli\u003eSupplied in 400ml aerosols\u003c\/li\u003e\n\u003cli\u003e\n\u003ctable border=\"1\" cellspacing=\"1\" cellpadding=\"1\"\u003e\n\u003ctbody\u003e\n\u003ctr\u003e\n\u003ctd\u003e\u003cstrong\u003eDrying Time\u003c\/strong\u003e\u003c\/td\u003e\n\u003ctd\u003eUnder 2min @ 20°C\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003e\u003cstrong\u003eFlammability\u003c\/strong\u003e\u003c\/td\u003e\n\u003ctd\u003eNon-Flammable\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003e\u003cstrong\u003eCarrier Fluid\u003c\/strong\u003e\u003c\/td\u003e\n\u003ctd\u003eDichloromethane\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003e\u003cstrong\u003ePropellant\u003c\/strong\u003e\u003c\/td\u003e\n\u003ctd\u003eCarbon Dioxide\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003e\u003cstrong\u003eTemperature Range\u003c\/strong\u003e\u003c\/td\u003e\n\u003ctd\u003e5 to 50°C\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003e\u003cstrong\u003eShelf Life\u003c\/strong\u003e\u003c\/td\u003e\n\u003ctd\u003eAerosol - 18 Months\u003cbr\u003eBulk - 36 Months\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003c\/tbody\u003e\n\u003c\/table\u003e\n\u003c\/li\u003e\n\u003c\/ul\u003e","brand":"Foster Industrial","offers":[{"title":"Default Title","offer_id":52837382783307,"sku":"52250","price":19.06,"currency_code":"GBP","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0944\/6994\/7723\/files\/52250.jpg?v=1752153644"},{"product_id":"neocol-b-black-magnetic-ink","title":"Neocol B Black Magnetic Ink Aerosol 400 ml","description":"\u003cp class=\"large\"\u003e\u003cstrong\u003eJohnson \u0026amp; Allen's black magnetic ink easily detects weld defects.\u003c\/strong\u003e\u003c\/p\u003e\n\u003cul\u003e\n\u003cli\u003eSuspended high quality magnetic particles formulated to offer defined indications.\u003c\/li\u003e\n\u003cli\u003eIdeal for the inspection of welds, pressure vessels, structures, pipes, castings and forgings.\u003c\/li\u003e\n\u003cli\u003ePropels at a ratio far superior to liquid propellants such as Butane.\u003c\/li\u003e\n\u003cli\u003e400ml aerosol.\u003c\/li\u003e\n\u003cli\u003e\n\u003ctable border=\"1\" cellspacing=\"1\" cellpadding=\"1\"\u003e\n\u003ctbody\u003e\n\u003ctr\u003e\n\u003ctd\u003e\u003cstrong\u003eWhite Light\u003c\/strong\u003e\u003c\/td\u003e\n\u003ctd\u003e\u0026gt;500 Lux\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003e\u003cstrong\u003eFlash Point\u003c\/strong\u003e\u003c\/td\u003e\n\u003ctd\u003e\u0026gt;100°C\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003e\u003cstrong\u003eCarrier Fluid\u003c\/strong\u003e\u003c\/td\u003e\n\u003ctd\u003eIsoparaffin\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003e\u003cstrong\u003ePropellant\u003c\/strong\u003e\u003c\/td\u003e\n\u003ctd\u003eCarbon Dioxide\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003e\u003cstrong\u003eMethod\u003c\/strong\u003e\u003c\/td\u003e\n\u003ctd\u003eWet Method\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003e\u003cstrong\u003eType\u003c\/strong\u003e\u003c\/td\u003e\n\u003ctd\u003eNon-Fluorescent \/ Visible\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003e\u003cstrong\u003eTemperature Range\u003c\/strong\u003e\u003c\/td\u003e\n\u003ctd\u003e5 to 50°C\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003e\u003cstrong\u003eShelf Life\u003c\/strong\u003e\u003c\/td\u003e\n\u003ctd\u003eAerosol - 18 Months\u003cbr\u003eBulk - 36 Months\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003e\u003cstrong\u003eStandards\u003c\/strong\u003e\u003c\/td\u003e\n\u003ctd\u003eISO 9934\u003cbr\u003eASTM E1444\u003cbr\u003eASTM E709\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003c\/tbody\u003e\n\u003c\/table\u003e\n\u003c\/li\u003e\n\u003c\/ul\u003e","brand":"Foster Industrial","offers":[{"title":"Default Title","offer_id":52837401067851,"sku":"52255","price":16.56,"currency_code":"GBP","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0944\/6994\/7723\/files\/52255_1.jpg?v=1752153681"},{"product_id":"neopaint-2-white-contrast-paint","title":"Neopaint 2 White Contrast Paint Aerosol 400 ml","description":"\u003cp class=\"large\"\u003e\u003cstrong\u003eNeopaint 2 is a quick drying white contrast aid paint that has been specifically formulated for use in MPI. \u003c\/strong\u003e\u003c\/p\u003e\n\u003cp class=\"large\"\u003e-Johnson \u0026amp; Allen contrast paints produce a uniform and solid white background using formulations high in Titanium Dioxide.\u003c\/p\u003e\n\u003cp\u003e-Neopaint 2 is suitable for use with both aqueous and Hydrocarbon based consumable products and can be used in conjunction with either black or red magnetic inks.\u003c\/p\u003e\n\u003cp\u003e-400 ml\u003c\/p\u003e","brand":"Foster Industrial","offers":[{"title":"Default Title","offer_id":52837953569099,"sku":"52233","price":18.0,"currency_code":"GBP","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0944\/6994\/7723\/files\/52233.jpg?v=1752154460"},{"product_id":"chemetall-wcp-712-white-contrast-paint","title":"Chemetall WCP 712 White Contrast Paint -400ml","description":"\u003cp\u003e\u003cstrong\u003eChemetall Supramor WCP 712 White Contrast Paint, in a 400 ml aerosol.\u003c\/strong\u003e\u003c\/p\u003e\n\u003cul\u003e\n\u003cli\u003eWCP712 White Contrast Paint is a quick drying white paint, which is designed specifically for use in the colour contrast method of magnetic particle inspection.\u003c\/li\u003e\n\u003cli\u003eProvides a dense white background against which black or red indications of defects can be seen.\u003c\/li\u003e\n\u003cli\u003eIdeal for use with Supramor 4 Black magnetic ink.\u003c\/li\u003e\n\u003c\/ul\u003e","brand":"Foster Industrial","offers":[{"title":"Default Title","offer_id":52842178806091,"sku":"522112","price":15.01,"currency_code":"GBP","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0944\/6994\/7723\/files\/wcp712.png?v=1752160297"},{"product_id":"chemetall-ardrox-800-black-magnetic-ink","title":"Chemetall Ardrox 800\/3 Black Magnetic Ink- 400 ml","description":"\u003cp\u003e\u003cstrong\u003eChemetall Ardrox 800\/3 Black Magnetic Ink, is a high sensitivity black magnetic ink used in non-destructive testing.\u003c\/strong\u003e\u003c\/p\u003e\n\u003cul\u003e\n\u003cli\u003eUsed on mild steel \u0026amp; low alloy steels for revealing surface defects.\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003cp\u003e \u003c\/p\u003e","brand":"Foster Industrial","offers":[{"title":"Default Title","offer_id":52842185130315,"sku":"522113","price":15.22,"currency_code":"GBP","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0944\/6994\/7723\/files\/522113_1.png?v=1752160306"},{"product_id":"chemetall-ardrox-9d1b-developer-400mls","title":"Chemetall Ardrox 9D1B Developer 400 ml","description":"\u003cp\u003e\u003cstrong\u003eChemetall Ardrox 9D1B Developer in 400 ml aerosol is a liquid suspension of an inert white powder in a quick drying solvent.\u003c\/strong\u003e\u003c\/p\u003e\n\u003cul\u003e\n\u003cli\u003eLow sulphur, halogen \u0026amp; alkali metal content\u003c\/li\u003e\n\u003cli\u003eUsed as a developer in penetrant testing of forged parts, welds cast \u0026amp; forged parts.\u003c\/li\u003e\n\u003c\/ul\u003e","brand":"Foster Industrial","offers":[{"title":"Default Title","offer_id":52842194534731,"sku":"522130","price":13.95,"currency_code":"GBP","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0944\/6994\/7723\/files\/522130b.png?v=1752160314"},{"product_id":"chemetall-ardrox-9pr5-cleaner-400mls","title":"Chemetall Ardrox 9PR5 Cleaner - 400 ml","description":"\u003cp\u003e\u003cstrong\u003eChemetall Ardrox 9PR5 Cleaner 400 ml aerosol is non chlorinated solvent used to remove excess penetrant.\u003c\/strong\u003e\u003c\/p\u003e\n\u003cul\u003e\n\u003cli\u003eLow sulfur \u0026amp; halogen content\u003c\/li\u003e\n\u003cli\u003eIdeal for the removal of oil, grease and other organic contamination\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003cp\u003e \u003c\/p\u003e\n\u003cp\u003e \u003c\/p\u003e","brand":"Foster Industrial","offers":[{"title":"Default Title","offer_id":52842198925643,"sku":"522131","price":12.56,"currency_code":"GBP","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0944\/6994\/7723\/files\/522131.png?v=1752160322"},{"product_id":"chemetall-ardrox-906a-penetrant","title":"Chemetall Ardrox 906A Penetrant 400 ml","description":"\u003cp\u003e\u003cstrong\u003eChemetall Ardrox 906A Penetrant in 400 ml aerosol spray is a visible light inspection penetrant.\u003c\/strong\u003e\u003c\/p\u003e\n\u003cul\u003e\n\u003cli\u003eUsed in non destructive testing for the detection of defects such as cracks, laps, cold shuts, weld porosity, casting \u0026amp; weld discontinuties.\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003cp\u003e \u003c\/p\u003e","brand":"Foster Industrial","offers":[{"title":"Default Title","offer_id":52842204135755,"sku":"522132","price":20.01,"currency_code":"GBP","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0944\/6994\/7723\/files\/522132-removebg-preview.png?v=1752160331"},{"product_id":"jac-2-cleaner-5-ltr","title":"JAC-2 Cleaner 5 Litre","description":"\u003cp class=\"large\"\u003e\u003cstrong\u003eJAC 2 dye penetrant cleaner \u0026amp; degreaser from Johnson \u0026amp; Allen.\u003c\/strong\u003e\u003c\/p\u003e\n\u003cul\u003e\n\u003cli\u003eCleans grease \u0026amp; dirt from the work piece, prior to the application of penetrant.\u003c\/li\u003e\n\u003cli class=\"large\"\u003eThen used as a Penetrant Remover, cleaner being applied by impregnating a lint free cloth and then wiping.\u003c\/li\u003e\n\u003cli\u003eUtlised during an inspection process, JAC 2 is applied by impregnating a lint free cloth to wipe away excess penetrant, prior to developer application.\u003c\/li\u003e\n\u003cli\u003e5 litre tin\u003c\/li\u003e\n\u003c\/ul\u003e","brand":"Foster Industrial","offers":[{"title":"Default Title","offer_id":52842692542795,"sku":"522102","price":78.8,"currency_code":"GBP","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0944\/6994\/7723\/files\/522102_1.jpg?v=1752161040"}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0944\/6994\/7723\/collections\/Weldcrack_Detection_Kits_Sprays_1.png?v=1761915747","url":"https:\/\/fosterindustrial.myshopify.com\/collections\/weld-crack-detection-kits-sprays.oembed","provider":"Foster Industrial","version":"1.0","type":"link"}